Polymer Property : Tensile Strength, Ultimate = 87700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 605 MPa

@Temperature 427 °C
87700 psi

@Temperature 801 °F
Haynes HR-160® alloy, hot rolled and solution annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Ultimate 605 - 655 MPa
87700 - 95000 psi
L direction
ArcelorMittal Speed 35-510 Electrical Steel
Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 605 MPa
87700 psi
Typical
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
Allegheny Ludlum AL 904 L™ Alloy (UNS N08904) is an austenitic stainless steel alloy designed for a middles to high level of corrosion resistance. The alloy is produced to low carbon levels for us..
Tensile Strength, Ultimate 605 MPa

@Temperature 760 °C
87700 psi

@Temperature 1400 °F
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..