Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.9 - 60.7 MPa
2600 - 8800 psi
Average value: 40.2 MPa Grade Count:86
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..