Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.16 MPa @Temperature 225 °C |
893 psi @Temperature 437 °F |
Air Aging, 70 hours; ASTM D412 Die C |
Freudenberg Simrit S50 Silicone Elastomer (VMQ) General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol.. |
|||
Tensile Strength, Ultimate | 6.16 MPa | 893 psi | |
Colorite Polymers Vinylbond 95-950-80 PVC Compound Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri.. |