Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.30 MPa | 1350 psi | ASTM D638 |
Multibase Multi-Flex® TPE A 8502 CLASSY GREY Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 15%. Multi-Flex TPE contains Krato.. |
|||
Tensile Strength, Ultimate | 9.30 MPa | 1350 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Trefsin® 3101-85 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |
|||
Tensile Strength, Ultimate | 9.30 MPa | 1350 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Trefsin® 3201-85 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Tensile Strength, Ultimate | 9.30 MPa | 1350 psi | ASTM D638-61T |
Chevron Phillips MarFlex® 1010 LDPE Extrusion Coating Resin
(discontinued **) Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che.. |
|||
Tensile Strength, Ultimate | 9.30 MPa | 1350 psi | |
Kuraray HYBRAR® Low Rebound Compound # 2 Control Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 9.30 MPa | 1350 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 5401 BLK Ash is 4.71%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 9.30 MPa | 1350 psi | ASTM D638-61T |
Chevron Phillips MarFlex® 1013 LDPE Extrusion Coating Resin Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che.. |
|||
Tensile Strength, Ultimate | 9.30 MPa | 1350 psi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 Radiator/Heater Hose FormulationNordel® IP 4570 |