Polymer Property : Tensile Strength, Ultimate = 96.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.58 - 96.5 MPa
1100 - 14000 psi
Average value: 48.2 MPa Grade Count:56
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..