Polymer Property : Transverse Strength = 29000 psi
Polymer Property :
Transverse Strength =
29000 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Transverse Strength
>=
200
MPa
>=
29000
psi
when destroyed
Voloknohim PA-SV30 Glass and Mineral Filled
Information provided by Voloknokhim