Polymer Property : Elmendorf Tear Strength TD = 1030 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 1030 g
1030 g
Dow ATTANE™ 4213 Ultra Low Density Polyethylene
ATTANE® 4213 copolymer is an ultra low density polyethylene that offers excellent flexibility, sealability, puncture resistance and superior strength. It exhibits oxygen transmission characteristic..