Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 40.8 g
40.8 g
ISO 6383-2
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene
EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse ..
Elmendorf Tear Strength TD 40.8 g
40.8 g
ISO 6383-2
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene
EX 6HT is a high density polyethylene with 1-Butene as co monomer. It has good toughness, low gel level, good tear strength, high tenacity.Applications: film extrusion, blending partner, refuse ba..
Elmendorf Tear Strength TD 40.8 g
40.8 g
ISO 6383-2
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene
EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending ..
Elmendorf Tear Strength TD 40.8 - 204 g
40.8 - 204 g
Average value: 99.4 g Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..