Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 499 g | 499 g | |
Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4201 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It complies with FDA reg.. |
|||
Elmendorf Tear Strength TD | 499 g | 499 g | |
Dow ATTANE™ 4601 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4601 copolymer is an ultra low density polyethylene blown film extrusion grade having high impact resistance and tear strength combined with improved softness, designed for use in medical p.. |
|||
Elmendorf Tear Strength TD | 499 - 1030 g | 499 - 1030 g | Average value: 674 g Grade Count:12 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |