Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 535 g | 535 g | ASTM D1922 |
NOVA Chemicals Surpass® FPs317-A Octene sLLDPE Film Resin Features: Exceptional puncture resistanceVery good tear propertiesLow gel levelExcellent optical properties Excellent elongation characteristics Easy to process, no drying required Applications: Cas.. |