Polymer Property : Elmendorf Tear Strength TD = 610 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 610 g
610 g
ASTM D1922
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin
Product Description: Enable 35-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Elmendorf Tear Strength TD 610 g
610 g
ASTM D1922
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 35-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..