Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 612 g
612 g
ASTM D1922
Eastman Tritan MP100 Copolyester
Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co..