Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 614 g | 614 g | ASTM D1922 |
Dow DOWLEX™ 2078G Linear Low Density Polyethylene Good processability at narrow die gaps High strength in food applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |