Elmendorf Tear Strength TD 620 g
620 g
ASTM D1922
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE
Notes: Terraloy™ BP-10001A is a Thermoplastic Starch/LLDPE ready-to-process compound that contains up to 30% of TPS renewable content. This compound is for blown film application. Forms: Pellets A..
Elmendorf Tear Strength TD 620 g
620 g
Modified rectangular test specimen; ASTM D1922
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP)
AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre..
Elmendorf Tear Strength TD 620 g
620 g
ASTM D1922
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su..