Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 674 g | 674 g | Method B; ASTM D1922 |
Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin General Purpose Resin Excellent Strength Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, de.. |