Polymer Property : Elmendorf Tear Strength TD = 975 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 975 g
975 g
ASTM D1922
Dow ELITE™ 5401G Enhanced Polyethylene Resin
™ 5401G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking for excellent performance on a..