Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 100 g/micron | 2540 g/mil | F50; ASTM D1709 |
Braskem BF 0323 HC LDPE Blown Film Extrusion Polyethylene Description: BF0323HC is a high molecular weight grade produced under high pressure. Films obtained with this product show excellent mechanical and optical properties38µm film gauge, obtained in 75.. |
|||
Dart Drop | 100 g/micron | 2540 g/mil | ASTM D1709 |
Braskem BF 0323/12 HC LDPE Blown Film Extrusion Polyethylene Description: BF0323/12 is a high molecular weight LDPE produced under high pressure technology. Films obtained with this product show outstanding optical properties, excellent mechanical properties,.. |