Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 4.45 g/micron | 113 g/mil | ASTM D1709 |
Westlake EMAC® EF598AA 9% Ethylene-Methyl Acrylate Copolymer Clarity optics, excellent drawdown, excellent machinability, good TD heat shrinkage and excellent toughness. Uses include food packaging tie layers, heat seal layers, extrusion coating, cast film, .. |
|||
Dart Drop | 4.45 g/micron | 113 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |