Polymer Property : Dart Drop = 134 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 5.28 g/micron
134 g/mil
ASTM D1709
Braskem ES 300 HDPE Blown Film Extrusion Polyethylene  (discontinued **)
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags; high-strength films. Informa..
Dart Drop 5.28 g/micron
134 g/mil
ASTM D1709
Huntsman Rexell® L8404 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, and FDA compliant.Applications: Blown film extrusion: general purpose.Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by H..