Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 5.91 g/micron | 150 g/mil | ASTM D1709 |
ExxonMobil LL 3105.50 Premium High Strength Film Resin
(discontinued **) LL 3150.32 is a hexene copolymer LLDPE film resin for blown film. Films produced from this resin have excellent tensile and toughness properties, as well as improved stiffness. Combined with good dr.. |
|||
Dart Drop | 5.91 g/micron | 150 g/mil | ASTM D1709 |
Huntsman PE 1302 EVA Film Extrusion
(discontinued **) 3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu.. |
|||
Dart Drop | 5.91 g/micron | 150 g/mil | ASTM D1709 |
Huntsman PE1356 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Dart Drop | 5.91 g/micron | 150 g/mil | ASTM D1709 |
Westlake Hifor Xtreme SC74836 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme Polyethylene SC74836 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock and processing aid. Films.. |
|||
Dart Drop | 5.91 g/micron @Thickness 0.0254 mm |
150 g/mil @Thickness 0.00100 in |
ASTM D1709A |
Total Lumicene® mPE M 3410 EP HDPE Film Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and.. |
|||
Dart Drop | 5.90 g/micron | 150 g/mil | |
Dow DOWLEX™ 2071 Linear Low Density Polyethylene DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks.. |
|||
Dart Drop | 5.91 g/micron | 150 g/mil | ASTM D1709 |
Huntsman PE1335 EVA Film Extrusion
(discontinued **) 3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Dart Drop | 5.91 g/micron | 150 g/mil | ASTM D1709 |
Huntsman PE1345 EVA Film Extrusion
(discontinued **) 3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Dart Drop | 5.91 g/micron | 150 g/mil | ASTM D1709 |
Westlake Hifor Xtreme SC74859 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74859 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and high processing aid.Application/U.. |