Dart Drop 6.60 g/micron
168 g/mil
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2070D Polyethylene resin is a fully formulated linear low density polyethylene resin offering high strength and low gel properties for blown film food packaging applications. DOWLEX 2070D r..