Polymer Property : Dart Drop = 18.0 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 18.0 g/micron
457 g/mil
ASTM D1709A
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE
Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b..
Dart Drop 18.0 g/micron
457 g/mil
ASTM D1709A
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..