Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.63 g/micron | 66.8 g/mil | ASTM D1709 |
Eastman 1550F Film Polyethylene
(discontinued **) Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long.. |
|||
Dart Drop | 2.63 g/micron | 66.7 g/mil | ASTM D1709 |
Westlake EN923 Low Density Polyethylene Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa.. |
|||
Dart Drop | 2.63 g/micron | 66.8 g/mil | ASTM D1709 |
Braskem LHB 118/21 AF LLDPE Blown Film Extrusion Polyethylene Description: LHB118/21 AF is a LLDPE copolymer produced by Braskem. It is a ready-to-use product since it contains 10% LDPE. Its additive package was optimized to avoid blocking, even at low thickne.. |
|||
Dart Drop | 2.63 g/micron | 66.8 g/mil | ASTM D1709 |
Braskem LL 118/21 LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |