Polymer Property : Dart Drop = 20.0 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 0.787 g/micron
20.0 g/mil
F50; ASTM D1709
Total PPH 3575CC Polypropylene Homopolymer, Film Grade