Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 22.0 g/micron | 559 g/mil | F<sub>50</sub>, ASTM D1709/A |
NOVA Chemicals Novapol® TD-9022-D Super Hexene Film Resin Excellent dart impact, High strength, High toughnessApplications: Retail trash bagsAdditives: Process stabilizer, Slip/antiblockFilm properties are typical of blown film extruded at a blowup ratio o.. |
|||
Dart Drop | 22.0 g/micron | 560 g/mil | ASTM D1709 |
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin
(discontinued **) Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Dart Drop | 22.0 g/micron | 560 g/mil | ASTM D1709 |
ExxonMobil Exceed™ 1023CA Tough Premium Film Resin
(discontinued **) Exceed 1023CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Dart Drop | 22.0 g/micron | 559 g/mil | ASTM D1709A |
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile.. |