Mechanical Properties Metric English Comments
Dart Drop 1.00 g/micron
25.4 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Dart Drop 1.00 g/micron
25.4 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 14K1 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Dart Drop 1.00 g/micron
25.4 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Dart Drop 1.00 g/micron
25.4 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Dart Drop 1.00 - 4.00 g/micron
25.4 - 102 g/mil
Average value: 1.96 g/micron Grade Count:9
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film