Polymer Property : Dart Drop = 259 g/mil
Polymer Property :
Dart Drop =
259 g/mil
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Dart Drop
10.2
g/micron
259
g/mil
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.