Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 11.0 g/micron | 280 g/mil | ASTM D1709 |
Huntsman PE1501 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with excellent impact strength, good heat seal, and good clarity.Applications: Film extrusion: greenhouse film, heavy-duty packa.. |
|||
Dart Drop | 11.0 g/micron | 280 g/mil | ASTM D1709 |
Huntsman PE1753 EVA Film Extrusion
(discontinued **) 7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and .. |