Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.67 g/micron | 93.2 g/mil | ASTM D1709 |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Dart Drop | 3.67 g/micron | 93.3 g/mil | ASTM D1709 |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |