Mechanical Properties Metric English Comments
Dart Drop 3.80 g/micron
96.5 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Stretch Wrap, CoextrusionsProcessing Conditio..
Dart Drop 3.80 g/micron
96.5 g/mil
ASTM-D1709
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene
TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th..
Dart Drop 3.80 g/micron
96.5 g/mil
ASTM-D1709
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene
TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its ..