Polymer Property : Dart Drop = 355 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 14.0 g/micron
355 g/mil
ASTM D1709
Huntsman PE1651 EVA Film Extrusion  (discontinued **)
6.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with outstanding low temperature strength, excellent clarity, and good heat seal.Applications: Film extrusion: ice bags, liqui..