Polymer Property : Dart Drop = 4.09 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 4.09 g/micron
104 g/mil
F50; ASTM D1709
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
Dart Drop 4.09 g/micron
104 g/mil
ASTM D1709
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Dart Drop 4.09 g/micron
104 g/mil
ASTM D1709
ExxonMobil LL 1001x72 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Dart Drop 4.09 g/micron
104 g/mil
ASTM D1709
ExxonMobil LL 1001x74 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Dart Drop 4.09 g/micron
104 g/mil
ASTM D1709
ExxonMobil LL 1001x76 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Dart Drop 4.09 g/micron
104 g/mil
ASTM D1709
ExxonMobil LL 1001x59 Blown Film Resin  (discontinued **)
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Dart Drop 4.09 g/micron
104 g/mil
ASTM D1709
Chevron Phillips MarFlex® 7109CL LLDPE Blown Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..