Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop = 400 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 15.7 g/micron
400 g/mil
Blown Film at 1 mil; ASTM D-1709
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE  (discontinued **)
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a..
Dart Drop 15.7 g/micron
400 g/mil
ASTM D1709
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
Dart Drop 15.7 g/micron
400 g/mil
ASTM D1709A
Westlake Mxsten CV77518 Polyethylene Plastomer
Mxsten CV Plastomer CV77518 resin is a polyethylene plastomer designed for blown and cast film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a ve..
Dart Drop 15.7 g/micron
400 g/mil
ASTM D1709
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
Copyright © lookpolymers.com All Rights Reserved