Polymer Property : Dart Drop = 41.89 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 41.89 g/micron
1064 g/mil
ASTM D1709A
ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications
Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blo..