Mechanical Properties Metric English Comments
Dart Drop 45.3 g/micron
1150 g/mil
ASTM D1709
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..