Dart Drop 17.7 g/micron
450 g/mil
Blown Film at 1 mil; ASTM D-1709
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE  (discontinued **)
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a..