Polymer Property : Dart Drop = 467 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 18.4 g/micron
467 g/mil
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade
ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com..
Dart Drop 18.4 g/micron
467 g/mil
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade
ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati..