Mechanical Properties Metric English Comments
Dart Drop 5.04 g/micron
128 g/mil
F50; ASTM D1709
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o..
Dart Drop 5.04 g/micron
128 g/mil
ASTM D1709
Westlake EF602 Low Density Polyethylene
Westlake EF602 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize..