Dart Drop 5.795 g/micron
147.2 g/mil
ASTM D1709
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer
Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo..