Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 2.25 g/micron
57.1 g/mil
ISO 7765/1
Borealis Himod™ FT6273 LDPE for Film
Himod FT6273 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Dart Drop 2.25 g/micron
57.1 g/mil
ISO 7765/1
Borealis Himod™ FT6274 LDPE for Film
Himod FT6274 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..