Polymer Property : Dart Drop = 625 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 24.6 g/micron
625 g/mil
F50; ASTM D-1709
ExxonMobil Escorene® HD-7000F HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7000F exhibit excellent impact and toughness properties as well as high stiffness..
Dart Drop 24.6 g/micron
625 g/mil
F50; ASTM D-1709
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness...