Polymer Property : 1% Secant Modulus = 1145.8 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 7.9000 MPa
1145.8 psi
ASTM D790
Dow Engage® ENR 7467.00 Ethylene-Butene Copolymer
Description: ENR 7467.00 is a high performance ethylene-butene copolymer, offering superior impact properties for more demanding TPO applications. The polymer has very low crystallinity and is avail..