Mechanical Properties Metric English Comments
1% Secant Modulus 1258 MPa
182500 psi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® H5520 High Density Polyethylene
ApplicationsALATHON H 5520 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include house..
1% Secant Modulus 1258 MPa
182500 psi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® M5040 High Density Polyethylene
ApplicationsALATHON M 5040 is a copolymer with broad molecular weight distribution. This resin exhibits excellent color, low odor, and good processing stability. Typical applications for this res..