Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 13.0 MPa | 1890 psi | ASTM D790 |
LG Chemical LC670 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |