Polymer Property : 1% Secant Modulus = 3495.4 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 24.100 MPa
3495.4 psi
ASTM D790
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer
Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th..