Mechanical Properties Metric English Comments
1% Secant Modulus 423 MPa
61400 psi
ASTM D790
ExxonMobil LL 5202.09 Compounding Resin  (discontinued **)
LL 5202.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL 5202.09 makes for efficient blending with pigments, slip ..