Polymer Property : 1% Secant Modulus = 480 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 480 MPa
69600 psi
ASTM D638
SABIC R40039E Medium Density Polyethylene for Rotational Molding
Product Description: R40039E is a Medium Density Polyethylene grade designed to provide excellent mechanical properties with high rigidity, toughness, gloss and low warpage. R40039E is UV stabiliz..