Mechanical Properties Metric English Comments
1% Secant Modulus 800 MPa
116000 psi
ASTM D638
SABIC M200056 High Density Polyethylene for Injection Molding
Product Description: M200056 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow..