Mechanical Properties Metric English Comments
Shear Strength 0.00689 - 172 MPa
1.00 - 25000 psi
Average value: 20.5 MPa Grade Count:255
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Shear Strength 0.00689 MPa
1.00 psi
Overlap, Aluminum, RT cure for 2 hrs; ASTM D1002
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..