Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | <= 0.0689 MPa | <= 10.0 psi | Overlap, CRS/CRS after 7 days of Immersion in MEK |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | <= 0.0689 MPa | <= 10.0 psi | Overlap, CRS/CRS after 7 days of Immersion in Acetone |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |